Dagger's Dual-Core Laser: Removing the Coating and Creating the Anchor Profile in One Process
Getting the old paint off is only half of a recoating job. If new coating is going on, the steel usually needs a specified profile and a clean, contaminant-free surface, and that has traditionally meant a second step with an abrasive blaster.
The Netalux Dagger 4000 was built to fold those two steps into one.
Why the anchor profile matters
Many industrial coatings need some tooth on the steel to bond properly. A laser that strips the coating beautifully but leaves smooth metal underneath can leave you with a second surface-prep job before you can paint.
So a typical maintenance spec has at least two parts:
Remove the old coating, rust and contamination.
Leave the steel with the profile and cleanliness the new coating needs.
Each part gets checked separately. A pulsed cleaning laser can handle the first very well. Dagger is designed to handle both.
How Dagger works
Needle, Kamino and Jango are pulsed lasers that fire short bursts of energy. Dagger is different. It's a 4000 W continuous-wave laser with two beams in one:
a 1000 W Gaussian core: focused, concentrated energy at the centre
a 3000 W top-hat ring: an even band of energy around it
The operator can run the core alone, the ring alone, or both together. That's what gives Dagger its control. One part of the beam can do the heavy lifting on the coating, while the other conditions the exposed steel to build the profile. Netalux calls this technology DCL®, Dual Core Laser.
Because it's continuous-wave, comparing Dagger by pulse energy doesn't make sense. The useful numbers are power, beam shape, scan speed and heat input.
One process, not always one pass
Picture weathered steel with an old protective coating. The laser has to break down or lift that coating and get it captured by extraction. Once bare steel appears, the energy reaching it starts shaping the surface. With the core and ring set up as part of a qualified process, the goal is to clean and profile in the same programmed operation.
That doesn't mean every square centimetre is stripped and profiled in a single sweep. Depending on the coating and the steel, the process may involve different settings, overlap patterns or passes. We say "one process" with confidence. We only say "one pass" when a test on your material proves it.
What counts as a good anchor profile?
There isn't one universal number. Your coating spec usually names a target range and a measurement method, and the right profile depends on the coating system.
Be careful with roughness numbers. Ra is an average roughness value. On its own it doesn't describe peak-to-valley height or the full texture of a prepared surface. If your spec calls for replica tape, a stylus profilometer or a comparator, we'll use that method.
The ISO 8503 standards cover profile measurement on abrasive blast-cleaned steel, including comparators (ISO 8503-1) and stylus measurement (ISO 8503-4). They're useful reference points, but they were written for blasting. For a laser-prepared surface, agree on the measurement method with your coating supplier or project engineer up front.
And remember that profile isn't the only test. A surface with the right texture but leftover residue, salts or heat effects still isn't ready to coat.
Where Dagger makes sense
Large steel structures headed for recoating are the obvious fit, especially where staging a separate abrasive blasting step is difficult, messy or slow. Fabricated components, plant equipment, tight-access repairs and production lines with repeatable surface specs are all worth testing too. Dagger can be mounted on robots, cobots and crawlers for automated work.
Geometry matters. Flat plate is easy to scan and measure. Welds, edges, corners, flanges and complex shapes are harder. A process that profiles a flat coupon perfectly may behave differently at an edge, so test on representative parts.
What the trial needs to prove
Before: identify the coating layers and thickness where known, the steel grade and its condition. Agree on what has to come off and what (if anything) must stay.
During: record the core and ring settings, scan pattern, stand-off, travel speed and number of passes, so another operator on another shift can repeat the result. Measure the profile in several places, not just the best-looking patch.
After: pair profile readings with visual inspection and any cleanliness tests your spec requires. If the coating supplier or asset owner wants it, apply a test coat and check adhesion. A surface can hit its roughness target and still behave differently once coated.
And honestly: time the whole job, including masking, access, part handling, extraction, filter changes, inspection and rework. One machine doing two steps can be faster or slower than blasting depending on the site. The trial tells you which.
Which Netalux model?
If the job is… | Start with | What needs proving |
Weld or small-feature cleaning | Needle | Precision and finish |
Portable mixed coating removal | Kamino 300 | Performance and material compatibility |
Broad coating removal, no profile required | Jango | Coverage and substrate protection |
Coating removal plus a specified steel profile | Dagger 4000 | Profile, cleanliness and heat effects |
These are different jobs, not a ranking. See our equipment overview and portable lineup.
Don't skip the heat question
A continuous-wave laser can put a lot of heat into the work, especially with slow travel or repeated overlap. That's part of what makes profiling possible, and it's also why Dagger needs a qualified process. Thin sheet, precision-machined features, heat-treated parts and sensitive alloys won't tolerate what heavy carbon-steel plate will.
The trial should check for discolouration, melting, distortion and any roughness change outside the target area. Critical parts may need metallurgical review or engineering sign-off.
Dagger changes the surface on purpose. The line that matters is between controlled, specified modification and unwanted damage.
Limits
A result on one steel grade won't automatically repeat on another. Very thick or complex coating stacks may need extra passes or a different approach. Thin or heat-sensitive parts may not suit continuous-wave profiling at all. Some projects require the prep method itself to be qualified by the owner or coating manufacturer.
We don't quote a universal roughness result or a guaranteed one-pass rate without test data on your material.
Safety
Dagger is a Class 4 laser at 1064 nm. The risk assessment has to cover the direct beam, mirror-like and scattered reflections, high local power, fire risk and whatever the coating releases. You need eyewear rated for 1064 nm, barriers and interlocks, a controlled work area and proper fume extraction. The right eyewear and barrier ratings come out of that assessment, not a rule of thumb.
Old coatings can contain lead, chromates and other hazardous materials. No blasting media doesn't mean no hazardous dust. Choose extraction, respiratory protection and waste handling for the contaminant. We supply laser safety equipment and Laserversity training for planning a safe deployment.
Frequently asked questions
Is Dagger a pulsed laser?
No. It's a 4000 W continuous-wave laser with a 1000 W Gaussian core and a 3000 W top-hat ring, which can run separately or together.
Will Dagger always clean and profile in one pass?
No. One pass depends on the coating, the steel, the scan program and the profile you need. We prove it on your material before promising it.
Is an Ra reading enough to say the steel is ready to coat?
Usually not. Agree on the profile method, cleanliness tests and any coating qualification for the project.
Can Dagger work on aluminium or delicate parts?
That's case by case. Heat effects need careful testing before we'd recommend it.
How do we start a Dagger trial?
Send us the steel, the coating stack, the profile you need and how it will be measured. Book a demo, arrange a sample test, or call +1 (705) 805-2737.